Skip to main content
. 2020 Jun 30;12(7):1469. doi: 10.3390/polym12071469

Table 2.

Setting properties of the PMMA- based BCs containing MWCNTs, CS/MWCNTs, GO, CS/GO, and AG reinforcing agents.

Sample T Max (°C) Setting Time (sec) Ref.
PMMA/ functionalized MWCNTs (with 0.1 wt % MWCNTs) 68.53 ± 6 1712 ± 7 [80]
PMMA/MWCNTs (with 1 wt % MWCNTs) ≈57 ≈1100 [83]
PMMA/ MWCNTs-COOH (with 0.1 wt % MWCNTs) 70.50 ± 6.87 694.2 ± 16.74 [84]
PMMA-CS/MWCNTs (with 25 wt % CS/MWCNTs containing 2.5 wt % CS and 0.5 wt % MWCNTs) 58.10 ± 2.77 970.2 ± 48 [90]
PMMA/GO (with 0.1 wt % of GO) 79 1080 [95]
PMMA-CS/GO (with 25 wt % CS/GO containing 2 and 0.3 wt % CS and GO respectively) 62.3 ± 1.9 768 ± 20.4 [101]
PMMA/AG 38 ± 1 1320 ± 120 [104]