Experimental tests performed with 300 wt% LEO, MMT and 10 wt% of CPB.

Sample Code Dispersion Conditions Temperature (°C) LEO (wt%)
EO.WO_300 Open vessel, water Ambient/Room 300
EO.WC.T50_300 Closed vessel, water 50 300
EO.WC.T100_300 Closed, water * 100 300

* Water was used in the first step with CPB and MMT. No solvent was used for LEO addition to the clay paste.