Material Freq (GHz) Tuning Ability1 (%) Max Bias (V) Q2 Max keff2 (%) Reference
SrTiO3 5.87 fr:1 7.5 78(Qs) 2 [110]
BaTiO3 ~4 fr:1.3
fa:4.0
10 30 6.2 [108]
Ba0.25Sr0.75TiO3 ~4 fr:1.2
fa:0.8
10 120 0.5 [108]
Ba0.25Sr0.75TiO3 ~5 fr:0.9 25 250(Qs)
350(Qs-de)
[111]
Ba0.25Sr0.75TiO3 5.46 fr:2 50 50(Qs)
140(Qp)
4.4 [112]
Ba0.25Sr0.75TiO3 5.76 fr:3.8 25 130(Qs) 7.1 [113]
Ba0.25Sr0.75TiO3 5.46 fr:1.9 50 260(Qs-de) 3.5 [114]
Ba0.3Sr0.7TiO3 2.85 fr:2.4
fa:0.6
615
kV/cm
200(Qs)
120(Qp)
4.4 [109]
Ba0.5Sr0.5TiO3 5.45 fr:2.4 50 250(Qs-de) 7.5 [114]
Ba0.7Sr0.3TiO3 5.44 fr:1.3 6 352.6(Qs)
746(Qp)
17.15 [115]

1 Tuning ability at resonance frequency fr and antiresonance frequency fa. 2 Q-factor at series resonance Qs, parallel resonance Qp and series resonance after de-embedding Qs-de.