General procedure. (A) Microarray generation with laser induced forward transfer; (B) Spin-coating of donor slides (glass slide ≈1 mm, covered with self-adhesive polyimide foil, ≈75 um) with different polymer mixtures (e.g., polystyrene mixed with amino acid building block or fluorescent dye); (C) Melting and mixing of transferred polymer spots (not to scale). Reproduced with permission from [55].