Skip to main content
. 2020 Jul 17;12(7):1591. doi: 10.3390/polym12071591

Figure 4.

Figure 4

(a) The gas binding capacity of the a-PS(1.0) sensor as a function of binding time under the flow of three different gases (HCL, HF, and HCHO) at 100 ppm for a 25 min adsorption/desorption process and (b) the selectivity coefficient (k*) (Qe,HCl/Qe,(HF or HCHO) of HCl with respect to other gases.