Skip to main content
. 2020 Jul 20;5(30):19194–19201. doi: 10.1021/acsomega.0c02624

Table 1. Properties of Potassium Hydroxide Impregnated Char Sorbents with Different K Contents.

sorbent breakthrough time (min) breakthrough sulfur capacity (mg S per g sorbent) theoretical sulfur capacity (mg S per g sorbent) conversion of sorbent (%)
Char 118 114.20    
K5 104 124.22 205.10 56.18
K10 185 206.01 410.30 27.44
K12 341 342.20 492.30 69.51
K15 197 217.12 615.40 21.08
K20 85 68.83 820.50 11.90