Figure 7.
Scratch behavior of titanium after annealing at: (a) 600 °C for 24 h, (b) 600 °C for 72 h, (c) 700 °C for 24 h, (d) 700 °C for 72 h, (e) 800 °C for 2 h, (f) 800 °C for 6 h (Fn—indenter load, Ft—resistance to indenter penetration, Pd—depth of indenter penetration under load, Rd—depth of indenter penetration after unloading).