Skip to main content
. 2020 Jul 8;13(14):3048. doi: 10.3390/ma13143048

Figure 12.

Figure 12

Microscopic photographs of the friction path formed on titanium after tests with Al2O3 balls (corrugation wear: (a) light grey zone, (b) dark grey zone).