Skip to main content
. 2020 Jul 10;13(14):3093. doi: 10.3390/ma13143093

Figure 2.

Figure 2

Dynamic light scattering (DLS)-measured hydrophobic diameter (HD) (a) and zeta potential (b) of purified Au nanoparticles (NPs) of different sizes after their exposure to cCCM for different times. Reprinted with permission from [10]. Copyright (2017) American Chemical Society.