UV–vis absorption spectra of MO exposed to different irradiation time in the presence of (a) pristine TiO2 and (b) TiO2@400-Fe2O3 catalysts under visible light irradiation. The inserts are the photos of MO solution before and after irradiation. (c) Visible light photocatalytic degradation curves of MO and (d) −In(C/C0) vs. time curves by using TiO2 with and without Fe2O3 coating as catalysts.