(a) Three cycles of MO degradation for TiO2@400-Fe2O3, TiO2@800-Fe2O3 and 20 cycles Al2O3 coated TiO2@400-Fe2O3 in 90 min. (b) Comparison of MO degradation curves for pristine TiO2, TiO2@400-Fe2O3, and 20 cycles Al2O3 coated TiO2@400-Fe2O3.