Skip to main content
. 2020 Aug 11;10:13507. doi: 10.1038/s41598-020-69032-9

Figure 8.

Figure 8

Photocatalytic degradation of AB113 (a) Adsorption and self-degradation plots along with the comparison of photocatalytic activity of TiO2, BiVO4 and the three nanocomposite ratios [AB113]0 = 40 mg/l, [nanocomposite, TiO2, BiVO4] = 1 g/l pH0 = 6. (b) [AB113]0 = 40 mg/l, [nanocomposite] = 1–5 g/l pH0 = 6 (c) Comparison of the activity of TiO2 (Both adsorption and photocatalysis).