Table 1.
Particle | Medium | d(H, Z-avg) (nm) |
PDI | ζ (mV) | pH | σ (mS/cm) |
---|---|---|---|---|---|---|
PC | dH2O | 867 | 0.200 | −29.8 | 6.13 | 0.012 |
AEGM | 1208 | 0.140 | −9.73 | 7.41 | 12.3 | |
SAGM | 801 | 0.372 | −12.7 | 7.48 | 12.2 | |
PC-CNT | dH2O | 541 | 0.048 | −35.5 | 6.31 | 0.010 |
AEGM | 701 | 0.175 | −9.85 | 7.42 | 12.2 | |
SAGM | 587 | 0.206 | −12.3 | 7.48 | 11.4 | |
PU | dH2O | 836 | 0.209 | −6.97 | 5.34 | 0.014 |
AEGM | 724 | 0.284 | −10.3 | 7.48 | 12.1 | |
SAGM | 579 | 0.371 | −10.7 | 7.50 | 11.6 | |
PU-CNT | dH2O | 603 | 0.233 | −7.47 | 5.31 | 0.015 |
AEGM | 559 | 0.375 | −9.21 | 7.53 | 12.1 | |
SAGM | 417 | 0.305 | −11 | 7.52 | 11.4 |
Incinerated thermoplastics were diluted to 0.1 mg/mL in respective medium and assessed for intensity-based hydrodynamic diameter [d(H, Z-avg)], polydispersity index (PDI), zeta potential (ζ), suspension pH, and suspension conductivity (σ)