Table 2.
Particle | Medium | ρagg (g/cm3) | d(Vol-weighted) (nm) | Deposition Efficiency |
---|---|---|---|---|
PC | AEGM | 1.023 | 1255 | 18.6% |
SAGM | 1.024 | 1288 | 17.4% | |
PC-CNT | AEGM | 1.023 | 976 | 10.8% |
SAGM | 1.028 | 792 | 8.2% | |
PU | AEGM | 1.021 | 1092 | 21.8% |
SAGM | 1.025 | 747 | 7.1% | |
PU-CNT | AEGM | 1.020 | 601 | 9.3% |
SAGM | 1.020 | 551 | 2.1% |
DLS measurements in AEGM and SAGM were combined with aggregate density (ρagg) derived from the volumetric centrifugation method, and volume-weighted hydrodynamic diameter (d(Vol-weighted)) in the Distorted Grid Model to derive the depositional efficiency of particle sedimentation into the in vitro cellular microenvironment averaged over a 72 h exposure