Skip to main content
. 2020 Jun 9;45(3):e35. doi: 10.5395/rde.2020.45.e35

Table 4. Push-out bond strength of the calcium silicate sealers in the articles included in this review.

Material (CS) Method Compared material Push-out bond strength
BioRoot RCS Single cone AH Plus (ER), GuttaFlow2 (silicone) AH Plus > BioRoot RCS > GuttaFlow 2 (Donnermeyer et al. [100])
Endoseal MTA No obturation AH Plus (ER), MTA Fillapex (CS) AH Plus > Endoseal MTA > MTA Fillapex (Silva et al. [101])
EndoSequence BC Lateral compaction, Thermoplasticized injection technology AH Plus (ER), MTA Plus Sealer (CS) AH Plus > EndoSequence BC sealer; lateral compaction > Thermoplasticized injection (Dabaj et al. [55])
Single cone, Continuous wave AH Plus (ER) EndoSequence BC sealer = AH Plus > MTA Plus; Single cone > Continuous wave (DeLong et al. [51])
iRoot SP No obturation AH Plus (ER), EndoREZ (ER), Sealapex (CH) iRoot SP = AH Plus > EndoREZ = Sealapex (Ersahan and Aydin [102])
Single cone RealSeal SE (MR), AH Plus (ER), MTA Fillapex (CS) AH Plus = iRoot SP > MTA Fillapex > RealSeal SE (Nagas et al. [50])
BioRoot RCS No obturation TotalFill BC (CS), AH Plus (ER), Endo CPM (CS) AH Plus > TotalFill BC Sealer > BioRoot RCS > Endo CPM Sealer (Donnermeyer et al. [20,21])

CS, calcium silicate; ER, epoxy resin; CH, calcium hydroxide; MR, methacrylate resin.