Figure 28.

Figure 28

Thermal stability of the Al84Ni7Gd6Co3 (at.%) alloy, produced by a combination of gasification, ball milling and hot pressing as compared to other alloys taken from the literature. HP0—hot pressing at 640 MPa and THP = 500 °C using gas-atomized powders; HP2—powders milled for 50 h (HP1) and 100 h [25].