Skip to main content
. 2020 Jul 28;13(15):3346. doi: 10.3390/ma13153346

Figure 7.

Figure 7

(ac) Inverse pole figure (IPF) maps and (df) grain boundaries (GB) maps of the ECAR-CB-A AZ31 Mg alloy samples prepared at different final rolling temperatures: (a,d) 350 °C, (b,e) 450 °C and (c,f) 550 °C.