Comparison of chemiresistive gas sensors performance based on graphene/PPy nanocomposites.

Target Gas Sensing Material Response LOD
Response Time Recovery Time Nanocomposite Preparation Method Ref.
NO2 RGO/Polypyrrole (PPy) 32%
(50 ppm)
- - - In situ polymerization [135]
Humidity RGO/PPy 138% - 15 s 20 s [131]
NH3 TiO2@PPy–GN 102.2%
(50 ppm)
1 ppm 36 s 16 s [77]
CO Na-X/rGO/PPy 14.9%
(5 ppm)
- 600 s 358 s [134]