Skip to main content
. 2020 Aug 3;53(16):7009–7024. doi: 10.1021/acs.macromol.0c01031

Table 2. Characteristics of Spontaneously Crosslinked Micelles Prepared from Different Polymers at a Polymer Concentration of 4 mg/mL.

entrya polymers Z-ave (nm)b PDI absorbance changec
2 p(CL9-DTC3.9)-PEG 18 ± 1 0.11 ± 0.03 18 ± 2%
6 p(DTC3.8-b-CL9)-PEG 18 ± 1 0.10 ± 0.05 18 ± 2%
9 pCL9-PEG 17 ± 1 0.15 ± 0.06 n.a.d
13 p(CL9-DTC6.6)-PEG 18 ± 0 0.07 ± 0.02 17 ± 3%
14 p(CL18-DTC7.5)-PEG 22 ± 2 0.09 ± 0.02 20 ± 2%
a

Entries in this table correspond to those listed in Table 1.

b

Z-average diameter of the micelles in PBS was measured by DLS after nanoprecipitation and dialysis (n = 3).

c

Relative decrease in absorbance at λ = 326 nm.

d

Not applicable.