Skip to main content
. 2020 Aug 5;12(8):1750. doi: 10.3390/polym12081750

Table 1.

Onset degradation temperatures (°C) and the maximum DTG peak temperature (°C) for PP and WPCs before and after recycling.

Recycling Tonset (°C) DTGmax (°C)
PP WPC PP WPC
0 440 292 460 469
1 438 287 459 467
3 435 287 457 465
5 435 287 458 469
7 434 286 457 468
9 434 286 456 469