. 2020 Jul 27;12(8):1664. doi: 10.3390/polym12081664

Figure 13.

Figure 13

The pictures of PVA/CNW (30% CNWs, 1% GA) hydrogels (ac) and pure PVA hydrogels (df) compressed by a thumb. (g) Release activities of BSA from the hydrogels at 25 °C [79].