L-PEI 5k and branched PEI of MW 1.3 kDa (B-PEI 1.3k) were crosslinked with 30% TAC. Zeta potential and hydrodynamic diameter of polymers as 0.1% aqueous dispersions were evaluated.

Entry PEI Mol% Crosslinker ζ Potential [mV] DH [nm]
V 5 kDa linear 0 n/a n/a
VI 5 kDa linear 30 11 109
VII 1.3 kDa branched 0 n/a n/a
VIII 1.3 kDa branched 30 17 101