Skip to main content
. 2020 Aug 17;12(8):1841. doi: 10.3390/polym12081841

Table 1.

Sintering parameters adopted to process the nanocomposite powders (thermoplastic polyurethane (TPU)/multi-walled carbon nanotubes (MWCNTs) and TPU/(MWCNTs-graphene (GE))).

Process Parameters Value
Laser power (W) 14
Laser scan spacing (μm) 200
Laser scan speed (pps) 40,000
Part bed temperature (°C) 85
Outline laser power (W) 5.6
Layer thickness (μm) 100