Figure 11.

Figure 11

Morphology of the PEEK tensile samples printed at different nozzle temperatures (left), and SEM micrographs of tensile fracture surface of printed PEEK at different printing temperatures: (a) 370 °C, (b) 380 °C, (c) 390 °C, and (d) 420 °C [96].