Skip to main content
. 2020 Aug 13;9(8):1117. doi: 10.3390/foods9081117

Table 4.

Thickness, tensile properties and hydrophobicity of the clove oil composite films.

Film Thickness (µm) Tensile Strength (TS (MPa)) Elongation at Break (EB (%)) Water Contact Angle (WCA (Degree))
PLA/PBAT 36.71 ± 4.58 a 1.35 ± 0.03 c 5.63 ± 0.41 a 61.61 ± 2.82 a
PLA/PBAT-Clove1% 46.67 ± 3.59 a 0.94 ± 0.08 b 39.97 ± 0.09 d 62.24 ± 5.75 a
PLA/PBAT-Clove5% 73.33 ± 7.07 b 0.89 ± 0.06 a, b 27.58 ± 0.36 c 64.69 ± 2.15 a
PLA/PBAT-Clove 10% 106.67 ± 16.68 c 0.79 ± 0.03 a 25.67 ± 0.52 b 74.74 ± 4.11 b

The letters (a–d) at each concentration specifies groups that are significantly different (p < 0.05).