Skip to main content
. 2020 Aug 18;10(8):1614. doi: 10.3390/nano10081614

Figure 1.

Figure 1

(a) Thermal analysis of the cerium oxalate precursor (total theoretical weight loss is 52.49%). (b) XRD pattern recorded at room temperature for CeO2 nanoparticles (nps).