Figure 7.

Figure 7

Catalytic activity of the metal-wool electrodes as function of the run number. Reaction conditions: applied voltage = 5 kV; frequency 50 kHz; electrode length = 150 mm; wool-like metal = 61.3 cm2; flow rate = 100 mL min−1; H2/N2 = 1 [34]. Adapted with permission from Masakazu Iwamoto, Mao Akiyama, Keigo Aihara, et al., ACS Catalysis; published by American Chemical Society, 2017.