. 2020 Aug 17;13(16):3642. doi: 10.3390/ma13163642

Figure 8.

Figure 8

SEM images of steel rebar samples after 120 h of exposure in (a) bare (SCP + 3.5 wt.% NaCl) and (b) 2% inhibitor-added SCP + 3.5 wt.%% NaCl solution, at 1000×.