Comparison between experimental and predicted σFU and lower σBL strength for self-healing ceramics including various SiC healing agents. (a) AS30P [1] healed at 1573 K, 1473 K, and 1373 K in air and (b) monolithic SiC healed for 1 h and 10 h in air. (c) Effect of crack length on strength for AS30P [2] healed at 1573 K for 1 h in air and (d) effect of crack length on strength AS30 W [2] at 1,573 K for 1 h and 10 h in air.