Skip to main content
. Author manuscript; available in PMC: 2021 Aug 3.
Published in final edited form as: Angew Chem Int Ed Engl. 2020 Jun 3;59(32):13430–13436. doi: 10.1002/anie.202004098

Table 1.

Resistance values determined by 4-point probe of hydrated and dehydrated agarose hydrogels doped with different polymers.

+150 mM HBSS −150 mM HBSS

Resistance (ohms) Resistance (ohms)
Gel only 101.56 1.56 * 104
Hydrated Gel + PSS 98.43 [a] 0.487 * 104 [b]
Gel + poly(2c) 91.87 [a] 0.401 * 104 [b]

Gel only > 2 * 108 > 2 * 108
Dehydrated Gel + PSS > 2 * 108 > 2 * 108
Gel + poly(2c) 3.14 * 107 > 2 * 108
[a]

p < 0.001 by one-tail t-test

[b]

p < 0.005 by one-tail t-test.