Skip to main content
. 2020 Aug 24;117(36):21945–21952. doi: 10.1073/pnas.2003869117

Fig. 3.

Fig. 3.

Decomposed amplitude sweeps for the samples and model used in this study: (A) Carbopol, (B) Saramito model (Bingham version), (C) xanthan gum, (D) concentrated Ludox, (E) filled polymer, and (F) worm-like micelles. Green lines denote the slopes that lead to the dimensionless viscoplastic fragility number, as well the specific values for each material. The Saramito model parameters used here are σy=94Pa, G=460Pa, ηs=20Pas, and ηb=28Pas. (Model details can be found in SI Appendix.)