Fig. 2.

Fig. 2

FESEM image on the opposite side of the bigger of the two fragments (magnification 260×). The arrows indicate the fracture trigger. In ceramics the typical rupture mechanism is said to be brittle, as it is a fast, unstable and usually unstoppable process when triggered, unlike ductile rupture.