. 2019 Sep 16;9(11):9953–9963. doi: 10.1021/acscatal.9b02139

Figure 2.

Figure 2

HAADF-STEM images of (A, B) the 2Pt/ZrO2 catalyst calcined at 550 °C (2Pt/ZrO2-550) and (C) the same material after reduction at 250 °C (2Pt/ZrO2-550-R250). In image (A), the arrows point to the single atom Pt species.