Entry Material Pt loading/wt % Surface area/(m2/g) Pt particle size/nm
1 ZrO2 0 32 n.a.
2 0.5Pt/ZrO2-550-R250 0.6 n.d. 0.8
3 1Pt/ZrO2-550-R250 1.1 n.d. 1.2
4 2Pt/ZrO2-550-R250 2.1 29 1.4
5 5Pt/ZrO2-550-R250 4.8 n.d. 2.0
6 9Pt/ZrO2-550-R250 8.4 n.d. 2.6