Skip to main content
. 2020 Jun 29;13(15):3901–3910. doi: 10.1002/cssc.202000867

Figure 2.

Figure 2

Schematic of the different thicknesses and the corresponding growth‐limiting steps. For a charging current density of j=C/5 and an OCV of U 0=0.01 V our choice of parameters (see Supporting Information (SI), Table SI‐1) yields L tun=2.05 nm, L diff=25 nm, L mig=620 nm.