Table 2. Overview of the P10 Samples Investigated Herein: Metal Content as Determined by ICP-OES; Hydrogen Evolution Rate (HER) in a Solvent Mixture Consisting of Equal Volumes of H2O, MeOH, and TEA; Half-Lifetime of the Electron Polaron Decay as Observed via Transient Absorption Spectroscopy, Defined with Respect to the Signal Amplitude at 1 μs.

residual metal metal content (ppm) HER (μmol h–1 g–1) t50% (s)
Ni 4000 1897 2.3 × 10–2
Pd 2000 2825 1.3 × 10–3
Pd 7000 5332 1.5 × 10–4
Pd 27000 4906 5.0 × 10–5