Table 2. Young’s Modulus and Yield Strength for Native Wood, Delignified Wood, and Wood Aerogel.

  density [kg/m3] Young’s modulus [MPa] yield strength [MPa]
native wood 129 ± 2 295 ± 24 12.9 ± 0.9
delignified wood 90 ± 12 82 ± 32 3.9 ± 1.5
wood aerogel 79 ± 8 25 ± 13 1.2 ± 0.3