Skip to main content
. 2020 Aug 30;13(17):3834. doi: 10.3390/ma13173834

Figure 8.

Figure 8

(a) PDP (potentiodynamic polarization) curves and (b)corrosion rate of MAO-WE43 and GelMA/MAO-WE43 samples. 1#: MAO-WE43; 2#: 1GelMA/MAO-WE43; 3#: 5GelMA/MAO-WE43; 4#: 10GelMA/MAO-WE43; 5#: 15GelMA/MAO-WE43.