Skip to main content
. 2020 Sep 3;13(17):3899. doi: 10.3390/ma13173899

Figure 7.

Figure 7

SEM images of AAO—top view (upper row) and nanoconcaves left on aluminum surface after AAO dissolution (lower row) for the samples anodized for 7 h, at 5 °C, 300 V, five times in a row in the same 0.25 M malic acid solution; in the right corners of the SEM images presented in the upper row, photographs of the samples after anodization are shown (in grey frames).