Skip to main content
. 2020 Aug 27;13(17):3793. doi: 10.3390/ma13173793

Figure 3.

Figure 3

XRD pattern of ZnO/Ag nanocomposite with correlation with the wurtzite phase of ZnO adapted from Ref. [23] and the face-centered cubic (FCC) phase of Ag, adapted from reference [20].