Table 2.
FT-IR spectra data of the extracted and chemical treated fish tail palm fibre.
| Wavelength range (cm−1) | Possible assignment | Types of fibre |
Source | |||
|---|---|---|---|---|---|---|
| RFT | SFT1% | SFT5% | SFT9% | |||
| 3600–3000 | O-H stretching H-bonded alcohol, water, phenols | 3326 | 3322 | 3318 | 3314 | Cellulose, hemicellulose, lignin |
| 2500–3000 | C-H stretching vibration in cellulose and hemicellulose |
2924 | 2928 | 2927 | 2924 | Cellulose, hemicellulose |
| 2000–1693 | =CO stretching vibration of carboxylic acid and ester groups of hemicellulose | 1745 | 1754 | 1743 | 1744 | Hemicellulose |
| 1693–1607 | absorbed water | 1639 | 1643 | 1641 | 1637 | Water |
| 1607–1486 | aromatic C C stretching in lignin | 1588 | 1584 | 1586 | 1582 | Lignin |
| 1486–1395 | CH2 bending | 1460 | 1464 | 1460 | 1461 | Cellulose |
| 1395–1347 | C-H bending | 1376 | 1382 | 1372 | 1370 | Cellulose |
| 1347–1286 | aromatic C—O bending | 1313 | 1315 | 1313 | 1318 | Lignin |
| 1286–1184 | -CO stretching of acetyl group | 1242 | – | – | – | Lignin |
| 1140–912 | C-O stretching vibration in cellulose | 1029 | 1032 | 1029 | 1021 | Cellulose, hemicellulose, lignin |
| 912–840 | β-Glucosidic linkage in cellulose | 897 | 901 | 893 | 893 | Cellulose |