Table 1.

The chemical compositions (at.%) of master alloy (alloy) and C0.1-alloy (C-doped) and the Vickers micro hardness of both samples.

Sample C Mo Nb Re Ta W Hardness
100 gf 500 gf 2000 gf
alloy - 14.43 ± 0.17 22.74 ± 0.38 15.29 ± 0.09 26.66 ± 0.19 20.90 ± 0.19 6.451 ± 0.140 6.035 ± 0.303 5.400 ± 0.213
C-doped 0.06 14.32 ± 0.41 22.63 ± 0.54 18.12 ± 0.28 26.44 ± 0.32 18.43 ± 0.26 5.826 ± 0.104 5.905 ± 0.086 5.749 ± 0.203