. 2020 Sep 11;8:655. doi: 10.3389/fchem.2020.00655

Figure 6.

Figure 6

(A) Modulus measured at strain level 30% as a function of the number of compression cycles for the P5C10 composite (blue bars) and P10C10 composite (white bars), and (B) change in thickness of composites.