Skip to main content
. 2020 Sep 30;6(3):836–879. doi: 10.1016/j.bioactmat.2020.09.013

Fig. 8.

Fig. 8

(a) Optical micrographs of as cast Zn-0.34Mn and Zn-0.76Mn alloys, and EBSD microstructures of Zn-0.34Mn and Zn-0.76Mn alloys: (b) R1, 83.3% hot-rolling; (c) R2, 83.3% hot-rolling + 84.0% cold-rolling; (d) R3, 83.3% hot-rolling, annealing (200 °C × 2 h, air cooling), and 84.0% cold-rolling. (Reproduced with permission from Refs. [189]).