Skip to main content
. 2020 Aug 11;59(40):17691–17696. doi: 10.1002/anie.202007804

Figure 5.

Figure 5

Yields of products in 1,3‐butanediol dehydration at 300 °C and 1.4 h−1 WHSV over H‐ZSM‐5 (left) and H‐Al‐PST‐24 (right). The bulk Si/Al ratios of H‐ZSM‐5 and H‐Al‐PST‐24 are 95 and 200, respectively. A 10 wt % aqueous solution of 1,3‐butanediol was used as a feed.