Figure 2.

Figure 2

SEM characterization of photonic crystals prepared by self‐assembly of NCs from dispersions at concentrations of a)–c) 100 d)–f) 50 and g)–i) 10 mg mL−1. The concentration of NCs and ligands has a strong influence on the viscosity of the sample, altering the distribution of NCs along the surface. Isolated pillars are formed at low concentrations, while a residual layer of NCs is formed all over the sample at 100 mg mL−1.