Skip to main content
. 2020 Aug 21;10(9):1646. doi: 10.3390/nano10091646

Figure 2.

Figure 2

X-Ray Diffraction (XRD) pattern of Fe3O4-Au nanoparticles (NPs) (blue line) and reference patterns of magnetite (black bars; JCPDS 04-007-2718) and gold (red bars; JCPDS 00-004-0784).