Skip to main content
. 2020 Sep 18;10(9):1873. doi: 10.3390/nano10091873

Figure 4.

Figure 4

SEM images of CAB/ZnO hybrid nanostructures obtained by the dipping method after thermal treating at 240 °C in the air for 1 h ((a) and (b) for M1), and carbon/ZnO after thermally treating at 600 °C in N2 for 30 min ((c) and (d) for M1 (T)).