Skip to main content
. 2020 Sep 21;13(18):4189. doi: 10.3390/ma13184189

Figure 11.

Figure 11

(a) Fibre bent due to large crack width under alternating tension–compression loading; scanning electron microscope (SEM) images reveal (b) the form of damage for C100-NC-2000-05 and (c) ruptured section of the fibre for C100-HC-1000-09.