Table 3.
Test Series | Crack Width in Cyclic Stage (UO) [µm] |
Lower Reversal Point (UU) [mm] |
Displacement Increment Per Cycle (I) [µm] |
Number of Cycles [-] |
Number of Successfully Tested Specimens | |
---|---|---|---|---|---|---|
Start | End | |||||
R | - | - | - | - | - | 11 |
C40-NC-200 | 40 | 60 | 0.020 | 0.10 | 200 | 7 |
C40-MC-200 | −0.010 | 10 | ||||
C40-HC-200 | −0.025 | 10 | ||||
C40-NC-1000 | 0.020 | 0.02 | 1000 | 4 | ||
C40-MC-1000 | −0.010 | 10 | ||||
C40-HC-1000 | −0.025 | 10 | ||||
C40-NC-2000 | 0.020 | 0.01 | 2000 | 10 | ||
C40-MC-2000 | −0.010 | 10 | ||||
C40-HC-2000 | −0.025 | 10 | ||||
C100-NC-200 | 100 | 200 | 0.020 | 0.50 | 200 | 10 |
C100-MC-200 | −0.010 | 10 | ||||
C100-HC-200 | −0.025 | 9 | ||||
C100-NC-1000 | 0.020 | 0.10 | 1000 | 11 | ||
C100-MC-1000 | −0.010 | 11 | ||||
C100-HC-1000 | −0.025 | 10 | ||||
C100-NC-2000 | 0.020 | 0.05 | 2000 | 10 | ||
C100-MC-2000 | −0.010 | 8 | ||||
C100-HC-2000 | −0.025 | 8 |